625 713C Inconel Alloy Pipe
video

625 713C Inconel Alloy Pipe


GNEE Group offers Nickel Alloy Inconel 625 713C in a variety of forms, including:







ส่งคำถาม
คุยตอนนี้

ในฐานะซัพพลายเออร์และผู้ผลิตชั้นนำในประเทศจีน GNEE Steel นำเสนอผลิตภัณฑ์โลหะผสมนิกเกิล-ที่คุ้มค่า-

การแนะนำสินค้า

 

625 713C alloy Pipe video

Alloy 625 Seamless Pipe

Outside Diameter: 3-600mm

Wall Thickness: 0.5-30mm

Length: 0.5- 12 meter

713C Equivalent grades

• Inconel 713C
• DIN 2.4671
• UNS N07713
• NiCr13MoAl

625 Inconel Pipe Chemical Composition

C S Cr2 Al-Ti
- - - - - 20.0 - 58.0
0.10 0.50 0.50 5.0 0.015 23.0 0.40 -

Inconel 713C Round Bar Chemical Compositons:

%

C

S

713C

12.0

-

-

-

3.8

0.05

0.5

-

1.8

5.5

-

-

14.0

2.5

0.25

0.5

5.2

0.15

1.0

0.5

2.8

6.5

0.20

0.015

625 713C Inconel alloy Pipe

625 713C Inconel seamless alloy Pipe suppliers625 713C stainless steel Pipe dealer

625 This alloy has excellent corrosion resistance and oxidation resistance, both has good tensile properties and fatigue properties from low temperature to high temperature 980 degree , and has the ability to resist stress corrosion in salt spray atmosphere. Therefore, it can be widely used in the manufacture of aerospace engine parts, aerospace structural parts and chemical equipment, as well as in situations where it is in contact with seawater and subjected to high mechanical stress.
Inconel713C is a nickel-based precipitation hardening equiaxed crystal casting superalloy, with ' phase as the precipitation strengthening phase, and the service temperature is below 900 degree . The alloy has high creep strength, thermal and cold fatigue resistance and oxidation resistance. The alloy has simple composition, does not contain cobalt, and has a low density. It is usually used in the cast state.

625 713C Inconel Alloy Pipe

625 713C Inconel Alloy Pipe

625 713C alloy  Pipe factory

625 713C Inconel tubing for sale

 

 

 





Q: About the product price of 625 713C Inconel alloy Pipe?

 

No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China

 

+86-15824687445

 

ss@gneesteel.com

 

mmkelly1314

 

+86 15824687445

 

ป้ายกำกับยอดนิยม: 625 713c inconel alloy pipe, China 625 713c inconel alloy pipe suppliers, ท่อโลหะผสม, มาตรฐาน ASTM Inconel Alloy ASTM, ชิ้นส่วนแบริ่งอัลลอย, อุปกรณ์อัลลอยที่ไม่ได้, Inconel Alloy SS ท่อ, หลอดอัลลอยที่ไม่ได้

ส่งคำถาม

whatsapp

โทรศัพท์

อีเมล

สอบถาม